There are following points to pay attention to when using pellet machine:
1. First check whether the compression ratio of the ring die matches the raw material being processed. If the compression ratio of the ring die is too large, the resistance of the powder to pass through the die hole will be large, the particles will be too hard to press out, and the output will be small. The compression ratio of the ring die is too small and the particles are not formed when pressed out. You must re-select the compression ratio of the ring die and check the smoothness of the inner hole of the ring die and whether the ring die is out of round. Inferior ring die is because the inner hole of the ring die is rough and the ring die is out of round. As a result, the discharging resistance is large, the particles are not smooth, and the discharging is difficult, resulting in lower output. Therefore, a high-quality ring membrane must be used.
2. Do not add too many raw materials when the biomass pellet machine first starts running. During the running-in period, the general output of the new pellet machine is lower than the rated output, but after the running-in period, the output will reach its rated output. Yield.
3. Pay attention to the grinding of the wood pellet machine. Before the biomass pellet machine is officially put into use, it is very important to grind the wood pellet machine properly. This is because the ring mold pressing roller of the wood pellet machine is a heat treatment component. During the heat treatment process, there are some burrs in the inner hole of the ring die. , these burrs will hinder the movement and shaping of materials during the operation of the wood pellet machine.
4. If the ring die has been used for a period of time, you must check whether the taper hole on the inner wall of the ring die is worn and whether the pressure roller is worn. If the wear is serious, the ring die can be processed and repaired, and the worn taper hole must be re-countersinked. The pressure roller must be replaced if it is worn. Die taper hole wear has a great impact on output.